1. Úvod
The RESIONE TH-BJD Tough Resin is specifically engineered for 3D printing Ball-Jointed Dolls (BJD) and other articulated models. This 405nm UV-curing resin is compatible with LCD, DLP, and MSLA 3D printers. It offers exceptional wear resistance, scratch resistance, and maintains precise shapes, ensuring joints fit snugly without powdering from friction. The resin is formulated to be non-yellowing over time, preserving the original color of your prints. Its robust properties make models resistant to cracking, impact, and drops, even delicate parts during transportation.

Image: RESIONE TH-BJD Tough Resin bottle and a finely detailed printed BJD head, showcasing the resin's smooth finish.
2. Bezpečnostní informace
Always prioritize safety when handling 3D printing resin. Follow these guidelines:
- Podmínky prostředí: Use the resin in an environment with a temperature between 25-35°C (77-95°F).
- Větrání: Ensure adequate ventilation in your workspace. Avoid using resin in environments with strong ultraviolet light, such as near windows.
- Osobní ochranné prostředky (OOP): Always wear goggles, nitrile gloves, and a mask when handling resin to prevent skin and eye contact and inhalation of fumes.
- Accidental Contact:
- If resin splashes into your eyes, immediately rinse with plenty of clean water and seek medical attention.
- If resin spills on your skin, wash thoroughly with soap and water.
- Skladování pryskyřice:
- Store resin in a cool, dark place, away from direct sunlight.
- Uchovávejte mimo dosah dětí a domácích zvířat.
- If the resin will not be used for several days, seal it in an opaque container to prevent contamination.
- Do not mix used resin with unused resin to avoid contamination.
- Likvidace odpadu: Do not pour liquid resin directly into drains. Pour waste resin into a transparent container, add a small amount of water, and cure it under sunlight. Once solidified, filter and dispose of it as solid waste according to local regulations.
3. Nastavení
Proper setup is crucial for successful 3D printing with RESIONE TH-BJD Tough Resin.
- Příprava pryskyřice: Before use, heat the resin to 70°C (158°F) and shake thoroughly to ensure proper mixing of components.
- Prostředí tiskárny: Ensure your 3D printer is in a stable environment, free from vibrations and direct sunlight.
- Struktura podpory: BJD models often have large print sizes and weight. To ensure stability, it is necessary to use a sufficient support structure (adjust support tip diameter and central body diameter).
- Build Plate Placement: If planning a full-size print, it is recommended to place an appropriately sized backplane at the bottom of the model before printing.
- Nastavení tiskárny: Due to the high viscosity of TH-BJD resin (651-675 mPa.s), it is necessary to appropriately extend the retract wait time and light-off delay, and adjust the lift distance to ensure stable printing results. Refer to the "Printing Parameters Reference" section for detailed settings.

Image: Important considerations before printing, including support structure and build plate placement.
4. Provoz
Follow these steps for optimal printing results with RESIONE TH-BJD Tough Resin.
4.1 Printing Parameters Reference
The following table provides recommended printing parameters for various printer brands. These are general guidelines; fine-tuning may be required for your specific printer model and environmental conditions. Always refer to your printer's factory standard resin parameters as a baseline.
| Nastavení | Pryskyřice | Printer Brand / Resin | TH-BJD Ultra White / Cream Pink (50um) | TH-BJD Ultra White / Cream Pink (30um) | Washing & Post-Curing |
|---|---|---|---|---|---|
| Okolní teplota | 25-35 °C (77-95 °F) | 25-35 °C (77-95 °F) | Doba praní | ||
| Layer Height (um) | 50 | 50 | 30 | ≤ 5 min | |
| Spodní doba expozice (s) | A | 2.5 * A | 1.8 * A | Washing Agent | |
| Normální doba expozice (s) | B | B | 0.7 * B | 95% Alcohol or IPA | |
| Light Off Delay / Retract After Exposure (s) | D | D + 2 | D + 2 | Post-Curing Light Source | |
| Bottom Lift Distance (mm) | E | E + 2 | E + 2 | 40W | |
| Lift Height (mm) | F | F + 2 | F + 2 | Post-Curing Time | |
| Normal Layer Lift Speed (mm/min) | G | G | G | 10 minutes on each side | |
| Rychlost zatahování (mm/min) | H | H | H | ||
| Rychlost zatahování (mm/min) | I | I | I |
Note: The parameters for HeyGears printers are based on the factory standard resin parameters for successfully printed models (or the printer's default standard resin parameters).
4.2 Následné zpracování
- Odstranění podpory: It is recommended to remove support structures from the printed object before washing.
- Mytí: Printed models can be quickly washed. If the resin liquid is difficult to wash off the surface, adjust the normal exposure time, extend the static time before printing, and increase the light-off delay and lift distance. The surface should not feel sticky after washing.
- Po vytvrzení: After washing, cure the model using a 40W UV light source for 10 minutes on each side. For articulated models, focus on curing the joints during the post-curing stage to ensure ideal strength and functionality.
- Stabilita barev: If the printed object yellows during the post-curing process, place it in a ventilated area for 48-96 hours to gradually restore its original color.

Image: Smooth and stable molding results, highlighting fine details on a BJD head.

Image: Comparison demonstrating the easy washability and diluent resistance of TH-BJD resin versus other resins.
5. Údržba
Proper maintenance ensures the longevity of your printed objects and resin.
- Storage of Printed Objects: Store printed objects in a cool, ventilated place. In high-humidity environments, consider coating the surface of printed objects with paint to enhance moisture resistance.
- Transportation of Printed Objects: To ensure safe transportation, wrap printed objects with foam and use sealed packaging. For hollow printed objects, ensure they are thoroughly cleaned and completely cured before packaging and shipping to prevent residual resin from affecting the object.
- Resin Container Cleaning: After use, clean the resin vat and build plate thoroughly with IPA or a suitable resin cleaner.
6. Řešení problémů
This section addresses common issues encountered during 3D printing with RESIONE TH-BJD Tough Resin.
- Prints Not Sticking to Build Plate:
- Ensure the build plate is properly leveled and clean.
- Prodlužte dobu expozice dna.
- Verify ambient temperature is within the recommended range (25-35°C).
- Print Failures / Delamination:
- Check exposure times and adjust if necessary (refer to printing parameters table).
- Increase light-off delay to allow resin to settle.
- Ensure the resin is well-mixed before printing.
- Inspect the FEP film for damage or cloudiness.
- Models Yellowing After Curing:
- This can sometimes occur. Place the yellowed object in a ventilated area for 48-96 hours; the color should gradually return to normal.
- Difficulty Removing Supports:
- Consider using a heat gun to slightly soften the supports before removal, as suggested by user reviews.
- Adjust support settings in your slicer software (e.g., use spherical contact points).
- Resin Viscosity Issues (too thick):
- Ensure the resin is warmed to the recommended temperature before use.
- Increase light-off delay to compensate for slower flow.
For further assistance with printing issues, please contact RESIONE customer service for technical support.
7. Specifikace
Detailed technical specifications for RESIONE TH-BJD Tough Resin.
| Vlastnictví | Testovací standard | Cream Pink | Ultra bílá | Krémová bílá |
|---|---|---|---|---|
| Viskozita (25°C) | ASTM D4212-10 | 675 mPa.s | 661 mPa.s | 651 mPa.s |
| Hustota | ASTM D4052-22 | 1.13 g/cm³ | 1.13 g/cm³ | 1.129 g/cm³ |
| Srážení | ASTM D792-20 | 1.211 g/cm³ | 1.212 g/cm³ | 1.216 g/cm³ |
| Tvrdost Shore (D) | ASTM D2240-05 | 80D | 80D | 80D |
| Pevnost v tahu | ASTM D638-14 | 44.24 MPa | 45.85 MPa | 43.67 MPa |
| Modul tahu | ASTM D638-14 | 1.42 GPa | 1.47 GPa | 1.43 GPa |
| Prodloužení při přestávce | ASTM D638-14 | 17.77 % | 16.57 % | 17.26 % |
| Pevnost v ohybu | ASTM D790-10 | 76.25 MPa | 79.35 MPa | 79.71 MPa |
| Ohybový modul | ASTM D790-10 | 2.22 GPa | 2.28 GPa | 2.31 GPa |
| Vrubová Izodova rázová houževnatost | ASTM D256-10 | 17.77 J/m | 18.49 J/m | 17.46 J/m |
| Water Absorption (24h) | ASTM D570-22 | 1.25 % | 1.16 % | 1.22 % |
*The data above are typical values and may vary. All RESIONE experiments are conducted at 50%-60% humidity and 25°C. The actual performance of the resin or printed objects may decrease in different temperatures or humidity levels. The data above is for RESIONE brand materials only and does not imply that other similar types of materials will perform the same.
Všeobecné specifikace produktu
- Značka: RI RESIONE
- Číslo modelu produktu: TH-BJD
- Barva: Ultra White (Special White)
- Materiál: Pryskyřice
- Hmotnost položky: 1 kilogram
- Rozměry balení: 25.4 x 10.6 x 10.4 cm
- Zdroj napájení: AC (for printer, not resin)
- Příslušenství: Bottle, Liquid
- Baterie v ceně: Žádný
- Date First Available on Amazon.co.jp: 2024. 11. 21
8. Záruka a podpora
RESIONE TH-BJD Tough Resin comes with a 3-year warranty period.
For any printing issues or technical support, please contact RESIONE customer service. You can find contact information on the official RESIONE webwebu nebo prostřednictvím vaší nákupní platformy.
9. Další zdroje
Explore these official videos for more insights into RESIONE resin products and 3D printing techniques.
9.1 RESIONE Resin Features
Video: This video from RESIONE demonstrates the capability to print supports as fine as 0.1 mm diameter, highlighting the precision achievable with their resins.
9.2 RESIONE M68 Tough Resin Strength Test
Video: This RESIONE video showcases the strength of M68 Tough Resin, providing an indication of the durability you can expect from RESIONE's tough resin line.
9.3 RESIONE F39 Medical Grade Resin
Video: This RESIONE video highlights the F39 resin, which is suitable for medical purposes. While not directly TH-BJD, it demonstrates RESIONE's material capabilities.